Oțel pentru scule A2 | 1.2363 | X100CrMoV5 | SKD12 | Oțel BA2
Oțelul A2 este un oțel matrițat pentru prelucrare la rece cu performanțe echilibrate: călibilitate excelentă, duritate uniformă după călirea secțiunilor mari; Rezistență puternică la uzură, particulele de carbură întârzie uzura și prelungesc durata de viață; Tenacitate excelentă, rezistență la impact și fisuri minime în condiții de duritate ridicată; Procesabilitate bună, ușor de prelucrat în stare recoaptă, recuperează rapid rezistența ridicată după tratamentul termic, potrivit pentru ștanțare la rece, scule așchietoare și alte scenarii.
- fucheng steel
- China
- 1 lună
- 2000 tone/lună
- informație
- video
- descărcare
A2 TOOL STEEL
| Smelting and Manufacture Method: | LF+VD+Forged |
| Delivery Condition: | Annealed |
| Delivery hardness: | ≤229 HBS |
| UT Test Standard: | Sep 1921-84 Class3 D/d,E/e |


A2 STEEL GRADE COMPARISON AND CHEMICAL COMPOSITION COMPARISON
| Standard/Steel Grade | Chemical Composition(%) | ||||||
| C | Si | Mn | Cr | Mo | V | ||
| ASTM | A2 | 0.95~1.05 | 0.10~0.50 | 0.40~1.00 | 4.75~5.50 | 0.90~1.40 | 0.15~0.50 |
| DIN/W-Nr. | X100CrMoV5-1/1.2363 | 0.95~1.05 | 0.20~0.40 | 0.40~0.70 | 4.80~5.50 | 0.90~1.20 | 0.10~0.30 |
| JIS | SKD12 | 0.95~1.05 | 0.10~0.40 | 0.40~0.80 | 4.80~5.50 | 0.90~1.20 | 0.15~0.35 |
APPLICATION
A2 steel is suitable for plastic deformation tools for difficult to process materials, precision stamping dies, dies for cold forging, deep drawing and threading, high-speed blanking punches, stainless steel plate punches, etc.
A2 Tool Steel Characteristics
A2 tool steel is an air hardened tool steel with a wide range of applications. A2 steel has good toughness and blade sharpness retention. Its wear resistance is between O1 steel and D2 steel. After heat treatment, its hardness becomes very high, ranging from 57 to 62 HRC.
One of the advantages of A2 tool steel is its good toughness. This means that it is not easily broken or deformed when subjected to impact or vibration. This makes A2 tool steel very suitable for manufacturing tools that need to withstand high impact forces, such as hammers, punches, etc.
In addition, A2 tool steel also has good blade sharpness retention. This means that after a period of use, the blade can still remain sharp. This is very important for tools that require frequent use, as it can save time and labor.
Another advantage of A2 tool steel is its high wear resistance. This means that it can be used for a long time under harsh working conditions without wear or damage. This makes A2 tool steel very suitable for manufacturing tools that need to withstand high wear, such as drill bits, milling cutters, etc.
However, A2 tool steel also has some drawbacks. Firstly, it cannot improve hardness through heat treatment. This means that after a period of use, it may become soft and lose its original performance. Therefore, when using A2 tool steel to manufacture tools, it is necessary to pay attention to regular inspection and maintenance.
In short, A2 tool steel is a very excellent tool steel material. It has excellent toughness, blade sharpness retention, and wear resistance, and is suitable for manufacturing various types of tools. Although it has some drawbacks, these drawbacks do not affect its widespread application in the market. If you are looking for a high-performance tool steel material, A2 tool steel is definitely a good choice.
Oțelul de scule A2 este utilizat pe scară largă în industria hardware, cum ar fi întreținerea auto, fabricarea mecanică, electronică și alte domenii. În aceste domenii, oțelul de scule A2 este utilizat pentru fabricarea diferitelor tipuri de scule, matrițe și alte piese. De exemplu, în industria de întreținere auto, oțelul de scule A2 este utilizat pentru fabricarea diferitelor tipuri de chei, șurubelnițe și alte scule manuale; În industria de producție mecanică, oțelul de scule A2 este utilizat pentru fabricarea diferitelor tipuri de freze, burghie și alte scule așchietoare; În industria electronică și electrică, oțelul de scule A2 este utilizat pentru fabricarea diferitelor tipuri de clești, cleme și alte scule de prindere.
Pe scurt, oțelul de scule A2 este un material excelent pentru oțelul de scule. Are performanțe excelente și o gamă largă de aplicații. Dacă sunteți în căutarea unui material de oțel de scule de înaltă performanță care să vă satisfacă nevoile, oțelul de scule A2 este cu siguranță o alegere bună.